Panavia F 2.0 bonding to contaminated zirconia
Four surface cleaning methods were used after contaminating the ceramic surface: air abrasion with 50 mum Al(2)O(3) at 2.5 bar pressure for 15s, cleaning with 37% phosphoric acid for 60s once or ...