Microstructural and Electrical Properties of Cordierite ...
2016-8-10 · process in an 8 mm diameter tool (Hydraulic press Ring, P-14, Veb Thuringer). The applied pressure was 392 MPa and an amount of 0.3 g of powders was used for each pressed sample. The compacts were placed in an alumina boat and heated in a tube furnace (Lenton Thermal Design Typ 1600). The samples were two-step sintered: non-isothermal up to 1300 oC